Sorry for repost, but my registeration was mixed up.
My question is what do I do to get flexcote lite to level out on blank where I want to apply a waterslide decal? I applied the FC with part of a credit card after seeing suggestion here. It left some small wavy areas, so I went over it with a new camel hair brush. I then used heat gun, on low, to debubble and warm finish a litte to help g