SPONSORS
2024 ICRBE EXPO |
Glass Coat rod finish
Posted by:
Herb Knowlton
(---.dhcp.rclk.wi.charter.com)
Date: May 13, 2015 12:20PM
I have taken a few years off from building rods and have started again. I am getting ready to finish the wraps and the resin part of my Glass Coat has hardened. I have been able to get almost all to liquify by using a hot water bath on the bottle, and placing it on a heat register. Is this finish OK to use or should I get new finish?
Thanks, Re: Glass Coat rod finish
Posted by:
Tom Kirkman
(Moderator)
Date: May 13, 2015 12:47PM
It should be fine to use.
............. Re: Glass Coat rod finish
Posted by:
Herb Knowlton
(---.dhcp.rclk.wi.charter.com)
Date: May 13, 2015 01:40PM
Thanks, Tom
Herb Sorry, only registered users may post in this forum.
|