russ lloyd
Thanks Again guys, I'll see how this next one turns out.
Cheers
Russ
Forum: rodboard 1 year ago
russ lloyd
Thanks for the reply's peoples. Lots of info here. I did grind the roller guides to a fine point as I normally do. No change in how I apply the epoxy and adding heat to release the bubbles, I use a heat gun from a distance. The only difference may have been the epoxy being old. 16oz probably 2 years old at least and due to the cold weather, I warmed the epoxy in the microwave 5 secs at a time til
Forum: rodboard 1 year ago
russ lloyd
Flex Coat high build is the epoxy I use. And yes, it sounds very plausible about the layering, but I haven't had issues in the past?
Thanks for the prompt reply ????
Forum: rodboard 1 year ago
russ lloyd
Hi All,
just wondering if someone can shed some light on why the epoxy has shown tiny cracks at the start of the guide feet. It hast cracked all the way through, but will it?
I built a 50lb game rod. I put 2 coats of epoxy over the under binds then I double wrapped the roller guides with size D thread then epoxied at least 3 times over the entire rod.
So where did I go wrong, I've never ha
Forum: rodboard 1 year ago
russ lloyd
All good, I just odered some back issues from the Rodmaker mag. Will just take some time to get to Aus.
Thanks again for your help.
Forum: rodboard 1 year ago
russ lloyd
Hi all,
I've been searching the web to try and find some info on how to apply / make a leather to a foregrip for a game rod. I have made a couple in the past but just can't seem to get the rippling effect how I'd like it. The store-bought rods leather finish looks good, but I can't seem to replicate them.
Also with the leather strapping, does anyone know where you can get the leather that has